Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.305 GPa @Temperature 120 °C |
44.2 ksi @Temperature 248 °F |
ASTM D790 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 0.305 GPa @Temperature 120 °C |
44.2 ksi @Temperature 248 °F |
ASTM D790 |
BASF Capron® 8202 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 0.305 GPa @Temperature 120 °C |
44.2 ksi @Temperature 248 °F |
ASTM D790 |
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 0.305 GPa | 44.2 ksi | ASTM D790 |
Sumitomo Chemical ESPOLEX® WT515 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Flexural Modulus | 0.305 GPa @Temperature 120 °C |
44.2 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Flexural Modulus | 0.305 GPa @Temperature 120 °C |
44.2 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8202 PA6 (Dry) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Flexural Modulus | 0.305 - 5.50 GPa @Temperature -40.0 - 120 °C |
44.2 - 798 ksi @Temperature -40.0 - 248 °F |
Average value: 1.40 GPa Grade Count:8 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |