Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
Multibase Multi-Pro® 2010 M Polypropylene Mica Filled, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | Tangent; ASTM D790 |
RheTech Products T30P100-00 30% Talc Reinforced Polypropylene, Natural Applications: Headlamp housingsI/P componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | Tangent; ASTM D790 |
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black Applications: BracketsAir ductsConsolesWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company BS464 Specialty Polystyrene
(discontinued **) Features: Medium Impact Resistance, Good MoldabilityUses: PackagingProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
PolyOne Edgetek® PI-1000 Polyetherimide (PEI)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 2.89 GPa | 420 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN333MS Low Friction Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/6 L UV BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: UV Stabilizer and LubricantFeatures: LubricatedAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
Chase Plastics CP Pryme® N300HL (Dry) Nylon 6, Heat Stabilized, Lubricated, Recycled Content Features: Heat StabilizedLubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFRMPPCC-20 20% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
Clariant Renol PA101LRD-190 Nylon 66, General Purpose, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
Clariant Renol PA113C Nylon 66, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
Chesterton MRS 5 Metal Rebuilding System MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as we.. |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D-790 |
Axiall HR-5009 Rigid PVC, Molding Georgia Gulf HR-5009 is a rigid, fitting-grade PVC compound designed for hot runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which incl.. |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
Quantum Acetal-Homopolymer Information provided by Quantum Advanced Engineering Plastics |
|||
Flexural Modulus | 2.90 GPa | 420 ksi | Tangent; ASTM D790 |
RheTech Products M20P100-01A 20% Mica Reinforced Polypropylene, Black Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |