Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.76 GPa | 400 ksi | Tangent; ASTM D790 |
RheTech Products G13P100-724UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, NH220L Clear Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Nylene® 204 (HS) , Fast Cycle Nylon 6 Description: Nylene® 204 (HS) is a fast cycle, medium viscosity, nucleated nylon 6. 204 is UL approved and automotive approved. Information provided by Custom Resins.ALM, Nylene Canada, and Custom .. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Nylene® NX4528 Unfilled Nylon 6,6/6 Description: Nylene® NX 4528 is an unfilled specialty nylon. 4528 is FDA/NSF approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Pol.. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
PolyOne Geon™ CPVC MC550 Polyvinyl Chloride, Chlorinated (CPVC) Information provided by PolyOne |
|||
Flexural Modulus | 2.76 - 3.45 GPa | 400 - 500 ksi | Average value: 3.00 GPa Grade Count:8 |
Overview of materials for Polycarbonate, Aramid Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)
(Unverified Data**) Udel P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved aest.. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Firestone CLM200-001 Nylon 6 Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Techmer ES Electrablend® PC SS10 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: ConductiveInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | tangent; ASTM D790 |
Spartech PP5130 Talc Filled Homopolymer Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Techmer ES HiFill® PP GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Techmer ES HiFill® PP GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/6 Nylon 66 Availability: North AmericaForms: PelletsFeatures: Low ViscosityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Chase Plastics CP Pryme® N100L (DAM) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-10FG-Y950 10% Glass Fiber Reinforced, Lubricated Information provided by Asahi Thermofil |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | |
Abatron AboCast 8504-1 One-Component Epoxy AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications. |
|||
Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
PolyOne LubriOne™ ATH-05KV/000 Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |