Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.74 GPa | 397 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87358 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.74 GPa | 397 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87771 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.74 GPa | 397 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.74 GPa | 397 ksi | ASTM D790 |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Modulus | 2.74 GPa | 397 ksi | ASTM D790 |
Quadrant EPP PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |
|||
Flexural Modulus | 2.74 GPa | 397 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E7001 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7001 is 27-29; Geon E7456 is 40-49; Geon E7130 is 38-43; Geon E7370 is 26-31Information provided by PolyOne |
|||
Flexural Modulus | 2.74 GPa | 397 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 2-3120 BPLU 9H0017 20% Talc-Filled, UV Stabilized Polypropylene Block-Copolymer INNOPOL® CS 2-3120 BPLU 9H0017 is a 20% talc filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3120 BPLU 9H0017 is developed for producing injection molded au.. |
|||
Flexural Modulus | 2.74 GPa @Temperature 23.0 °C |
397 ksi @Temperature 73.4 °F |
EN ISO 178 |
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Flexural Modulus | 2.74 GPa | 397 ksi | ASTM Test |
BASF Ultramid® B3S Q661 PA6 (Dry) Ultramid B3S Q661 is a general purpose, PA6 resin for injection molding. |
|||
Flexural Modulus | 2.74 GPa | 397 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L6180 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.74 - 6.41 GPa | 397 - 930 ksi | Average value: 4.02 GPa Grade Count:19 |
Overview of materials for Polyimide, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app.. |