Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.30 GPa @Temperature 23.0 °C |
334 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D201 PBT Information provided by Polykemi AB |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 143R PC (Europe-Africa-Middle East) LEXAN 143R is a medium viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 143R is available in transparent, translucent and opaque colours. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 163R PC (Europe-Africa-Middle East) LEXAN 163R is a medium viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 163R is available in transparent, translucent and opaque colours. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD104R PC (Europe-Africa-Middle East) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE141R PC (Europe-Africa-Middle East) LEXAN FXE141R is a medium viscosity multi purpose UV stabilized grade for visual effects in ""energy"". The material contains a release agent to ensure easy processing. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HF1140R PC High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPS1S PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® IR1840 PC (Europe-Africa-Middle East) IR1840 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX2489D PC (Europe-Africa-Middle East) Lexan LUX2489D is a polycarbonate resin with high reflective properties, UV additive, medium viscosity, injection molding grade exhibiting low dust attraction. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Europe-Africa-Middle East) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® OQ4320 PC (Europe-Africa-Middle East) LEXAN OQ4320 is a medium viscosity grade with a UV cut-off up to 400 nm and a greater optical purity than standard grades. Fields of application for this material are optical lenses, f.i. in sunglas.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® PC2200R PC (Asia Pacific) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 950A PC (Europe-Africa-Middle East) LEXAN 950A is a high viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXE173R PC This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML3982 PC (Europe-Africa-Middle East) LEXAN ML3982 is an UV stabilized grade, with an excellent flow. It contains a release agent to ensure easy processing. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2mm/min; ASTM D790 |
Kingfa JH830T Flame Retardant PC Features:UL V-0 @ 2.4mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceTransparentApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInfor.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ISO 178 |
Mitsubishi Xantar® MX 1000 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2mm/min; ASTM D790 |
Kingfa LONOY 2200 HT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ISO 178 |
LyondellBasell Astryn EPKC10ZC Polypropylene Copolymer, Mineral Filled Key Features: medium high melt flow, very high modulus, UV-stabilized, mineral-filled polypropylene copolymer, very high rigidity, good impact resistance, good weatherability, good processabilityApp.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics PC1000 PC (Asia Pacific) PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics PC1000 PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics PC1000R PC (Asia Pacific) PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ASTM D 790 |
SABIC Innovative Plastics Noryl GTX CRN500 PPE+PA6 (Asia Pacific) Pa6 based unfilled GTX for Non-Auto marketThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Europe-Africa-Middle East) NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ISO 178 |
Polyram RamTough PZ126 Polycarbonate, Low Viscosity General purpose, low viscosity polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | ISO 178 |
Total PS CPDS 819 Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) 819 is a high impact brominated flame retardant polystyrene. A combination of high flow and high heat stability gives excellent processability and reduced cycle tim.. |
|||
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML3485 PC (Europe-Africa-Middle East) LEXAN ML3485 is a low viscosity grade exhibiting an improved ductility over standard polycarbonate grades at equal flow. |