Polymer Property : Flexural Modulus = 316 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Asia Pacific)
Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me..
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer
Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® EXL1484T PC Copolymer
Lexan* EXL1484T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in c..
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Asia Pacific)
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb..
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac..
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® BFL2000B PC (Asia Pacific)
Lexan BFL2000B resin is a Br- & Cl-free FR polycarbonate resin featuring high flow with balanced impact. It is available only in dark colors.
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo..
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC
Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability.
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East)
Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability.
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East)
F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only.
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU
LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber.
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific)
Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability.
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics XYLEX HX7409HP PC+POLYESTER
Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI)..
Flexural Modulus 2.18 GPa
316 ksi
ASTM D790
Styron PULSEâ„¢ EXT 200 PC/ABS Engineering Resin
Overview: High Heat, High Impact PC/ABS resin for injection molded automotive plating and painting trim applications.Information provided by Styron
Flexural Modulus 2.18 GPa
316 ksi
2mm/min; ASTM D790
Denka TP-801 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co..
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer
40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® EXRL0681 PC Copolymer
25 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.18 GPa
316 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXE1434T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me..
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific)
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Asia Pacific)
Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI)..
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific)
25 MFR LEXAN High Flow Ductile Copolymer
Flexural Modulus 2.18 GPa
316 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Europe-Africa-Middle East)
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized