Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 20.7 GPa | 3000 ksi | 1.3 mm/min; ASTM D790 |
PolyOne LubriOne™ SF-30CF/15T Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 20.7 GPa | 3000 ksi | ASTM D790 |
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Modulus | 20.7 GPa @Temperature 23.9 °C |
3000 ksi @Temperature 75.0 °F |
Dry; 325°F 2kpsi; ASTM D790 |
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Chopped Molding Compound Reinforced Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz.. |
|||
Flexural Modulus | 20.7 GPa @Temperature 23.9 °C |
3000 ksi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 7781 E-Glass Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |
|||
Flexural Modulus | 20.7 GPa | 3000 ksi | ASTM D790 |
PolyOne Edgetek® NN-40CF/000 - OBSOLETE Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 20.7 GPa | 3000 ksi | ASTM D790 |
PolyOne Edgetek® PS-30CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 20.7 GPa | 3000 ksi | ASTM D790 |
PolyOne Edgetek® PK-40CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 20.7 GPa | 3000 ksi | Lengthwise; ASTM D790 |
G-11 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Flexural Modulus | 20.7 GPa | 3000 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This .. |
|||
Flexural Modulus | 20.7 GPa | 3000 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Flexural Modulus | 20.7 GPa @Temperature 23.0 °C |
3000 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |
|||
Flexural Modulus | 20.7 GPa | 3000 ksi | ASTM D790 |
Clariant Renol PPSSP0008 Polyphenylene Sulfide, Carbon Fiber, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 20.7 GPa | 3000 ksi | ASTM D790 |
Clariant Renol PPA1100G60 Polyphthalamide, 60% Glass Fiber Data provided by Clariant Masterbatches |