Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.069 GPa | 300.1 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 2507 T NAT 25% Filler Content Polypropylene Moisture is less than 0.06%. Multi-Pro 2507 T Natural is designed for high impact and high flexural strength. It can easily be colored and is FDA approved.Data provided by Multibase. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 5012 C Black 50% Filler Content Polypropylene Data provided by Multibase. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-Pro® 5012 C Natural 50% Filler Content Polypropylene This product is well suited to fabricate non-glossy appliance parts, such as a vacuum cleaner canister. It replaces ABS at favorable cost performance characteristics.Data provided by Multibase. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | I.B., TAN, 0.5 in/min; ASTM D790 |
LyondellBasell SEQUEL® E3000 TPO Description: SEQUEL® E3000 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require toughness and dimensional stability. This extrusion.. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D790 |
Ineos Nova 5400 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D790 |
Ineos Nova 5404 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D790 |
Lucent Polymers CPP-230 Polypropylene, 30% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D790 |
Lucent Polymers CPP-340 Polypropylene, 40% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D790 |
Lucent Polymers PC/ABS-1211P Polycarbonate+ABS, Impact Modified, Platable, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D 790 |
MRC Polymers NAXALOYâ„¢ 770-BK272 ABS + PC Alloy Information provided by MRC Polymers Inc. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D 790 |
MRC Polymers NAXALOYâ„¢ 770-NT137 ABS + PC Alloy Information provided by MRC Polymers Inc. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D 790 |
MRC Polymers NAXALOYâ„¢ 770-NT172 ABS + PC Alloy Information provided by MRC Polymers Inc. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D 790 |
MRC Polymers SATRANâ„¢ 805 ABS Terpolymer, Impact Modified Information provided by MRC Polymers Inc. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | tangent; ASTM D790 |
Entec Hypro™ PPC-CC40 Natural Copolymer Polypropylene, 40% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | tangent; ASTM D790 |
Entec Hypro™ PPH-CC30 Natural Homopolymer Polypropylene, 30% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | tangent; ASTM D790 |
Entec Hypro™ PPH-T20 Homopolymer Polypropylene, 20% Talc Reinforced Information provided by Entec |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D790 |
Ineos Nova 5450 High Impact Polystyrene
(discontinued **) High impact, Good ESCRApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were determined on injection molded specimens at 23.. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D790 |
Ineos Nova 5500 High Impact Polystyrene
(discontinued **) Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio.. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | I.B., TAN, 0.5 in/min; ASTM D790 |
Solvay Engineered Polymers SEQUEL® E3000 HMS TPO
(discontinued **) Description: SEQUEL® E3000HMS thermoplastic olefinic elastomer (TPO) is designed for exterior and interior applications that require stiffness and durability. This extrusion-grade material is spec.. |
|||
Flexural Modulus | 2.069 GPa | 300.1 ksi | ASTM D790 |
Ineos Nova 5504 High Impact Polystyrene
(discontinued **) Good overall balance of properties, USP Class VIApplications: Audio cassettes and cartridges, Housewares, Toys, Structural foam, Machine housings, Window framesProperties were determined on injectio.. |