Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.04 GPa | 296 ksi | ISO 178 |
PolyOne Nymax™ 1308 A HS Natural Polyamide 66 (Nylon 66) The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range o.. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 4251R PPC+PC High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | ASTM D790 |
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880... |
|||
Flexural Modulus | 2.04 - 2.37 GPa | 296 - 344 ksi | ASTM D790M |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | ASTM D790 |
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | |
Kuraray SEPTON® CM1 Compatibilizer Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DX94375H PC LNP* LUBRICOMP* DX94375H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10 LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10 LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® 1101 PBT+PC (Asia Pacific) Unreinforced, opaque polycarbonate/polyester alloy. Excellent low temperature impact plus chemical resistance to automotive fluid.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® 5220 PBT+PC (Asia Pacific) Unreinforced, polycarbonate-based polymer blend, excellent chemical resistance and impact.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP (Asia Pacific) LNP* Thermocomp* MB006HS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP LNP* THERMOCOMP* MB006HS is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized, Healthcare. |
|||
Flexural Modulus | 2.04 - 2.37 GPa | 296 - 344 ksi | UV Postcure; ASTM D790M |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
Flexural Modulus | 2.04 - 2.37 GPa | 296 - 344 ksi | ASTM D790M |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS VP-11 ELG Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | ASTM D790 |
Braskem H 501 HC Bioriented Film Polypropylene Applications: High stiffness; barrier films for conversionInformation provided by Braskem |
|||
Flexural Modulus | 2.04 GPa | 296 ksi | 1% secant; ASTM D790 |
Braskem H 501 HC Injection Molding Polypropylene Description: H 501HC is a low melt flow rate homopolymer, designed for very high stifness aplications with good processability. This product exhibit excellent chemical resistance and barrier propert.. |