Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products FT5100-04 Thermoplastic Polyolefin, UV Stabilized, White Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products FT5250-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products FT5250-650UV Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products P100-00 Polypropylene, Natural Applications: Automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products T20P252-00 20% Talc Reinforced Polypropylene, Natural Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 30-1200 A Description: Homopolymer Polypropylene Nucleated with AntistaticInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.72 GPa @Thickness 3.20 mm |
250 ksi @Thickness 0.126 in |
At 1.27 mm/min, 1% secant, injection molded ASTM Type 1 specimen; ASTM D790A |
Pinnacle Polymers 1335 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
PolyOne Edgetek® PE-40MC/000 High Density Polyethylene (HDPE)
(discontinued **) Description/Features:Mica FilledInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM X Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Techmer ES HiFill® PA12 Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | tangent; ASTM D790 |
Spartech PP5210 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D 790 |
Styrolution Zylar 960 MBS ZYLAR 960 is an impact modified styrene acrylic copolymer that provides toughness equivalent to some grades of polycarbonate, good clarity and superior processing characteristics for demanding injec.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade Notes: High-Impact; Exceptional impact strength, especially at low temperatures; FMVSS Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Teknor Apex Monprene® MP 1056 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 4101N Staple Fiber and Injection Molding Polypropylene HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101N is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | 1% Secant; ASTM D790A |
Dow INSPIRE™ 117.00 Performance Polymer 117.00 Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistance, and clarity a.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem FT021N Homopolymer Polypropylene Description: Contact clarity, nucleated, high flexural modulus. Applications: Suggested uses include thermoforming, portion-controlled packaging, deli containers. Process: Thermoforming. This resi.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Arkema Group Solarkote® PB Acrylic For PVC/acrylic alloys Information provided by Arkema Group |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® GPA300X ABS Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc. |