Mechanical Properties Metric English Comments
Flexural Modulus 16.8 GPa
2440 ksi
ASTM D790
PolyOne Edgetek® X AS-40CF/000 Natural SE Acrylonitrile Butadiene Styrene (ABS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Modulus 16.8 GPa
2440 ksi
ASTM D790
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)  (Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Flexural Modulus 16.8 GPa
2440 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RCL36 is a compound based on PA 66 resin containing PTFE, Carbon Fiber. Added features include: Electrically Conductive, Internally Lubricated.
Flexural Modulus 16.8 GPa

@Temperature 100 °C
2440 ksi

@Temperature 212 °F
ISO 178
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Flexural Modulus 16.8 GPa
2440 ksi
GB/T 9341-2008
Sichuan Deyang Haton® hGR50 Polyphenylene Sulfide, Glass Fiber Reinforced
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Flexural Modulus 16.8 GPa
2440 ksi
ISO 178
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Dry
Information provided by Unitika Ltd.
Flexural Modulus 16.8 GPa

@Temperature 100 °C
2440 ksi

@Temperature 212 °F
ISO 178
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..
Copyright © lookpolymers.com All Rights Reserved