Mechanical Properties Metric English Comments
Flexural Modulus 1.56 GPa
226 ksi
13 mm/min; ASTM D790
PolyOne Trilliant™ HC X THC 1100 Natural Copolyester
Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri..
Flexural Modulus 1.56 GPa
226 ksi
ASTM D790
Ravago Manufacturing Americas Hysun™ 697 ASA
Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago
Flexural Modulus 1.56 GPa
226 ksi
1% secant; ASTM D790-02
Ipiranga Petrochem PH 1710 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Flexural Modulus 1.56 GPa
226 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY A3000LTH ABS
LNP* STAT-LOY* A3000LTH is a compound based on ABS resin. Added features of this material include: Transparent, Antistatic, Formulation Locked.
Flexural Modulus 1.56 GPa
226 ksi
ASTM Test
Styrolution Luran® S 797 SE ASA
Luran S 797 SE is an extrusion ASA grade with especially high notched impact strength, used for sheet and profile extrusions. The data representable is based on extruded sheet.Information provided ..
Flexural Modulus 1.56 GPa
226 ksi
ISO 178
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, Conditioned
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
Flexural Modulus 1.56 GPa
226 ksi
ASTM Test
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned)
Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c..
Flexural Modulus 1.56 GPa
226 ksi
ISO 178
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, Conditioned
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..