Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Nymax™ GF 1200 60 HS Black 22 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PK-30CF/10T Polyetheretherketone (PEEK), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 15.2 GPa @Temperature 149 °C |
2200 ksi @Temperature 300 °F |
ASTM D790 |
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCN3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | Tangent |
Premix Premi-Glas® 1200-50VE 1200-50 VE SMC
(discontinued **) Description: Premi-Glas® 1200-50 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Edgetek® SF-20CF/000 Polyphenylene Sulfide (PPS)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Edgetek® SF-47GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Techmer ES Electrafil® J-1/CF/20 Nylon 66, 20% Carbon Fiber Reinforced |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Techmer ES Electrafil® J-1/CF/30/TF/13/SI/2 Nylon 66, 30% Carbon Fiber, 13% PTFE, 2% Silicone |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/30 Polycarbonate, 30% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Techmer ES HiFill® PA6 1020 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Sumitomo Bakelite North America E 8940SG Electrical Encapsulation Grade Epoxy Mineral reinforced epoxy molding compound formulated for the encapsulation of electronic devices requiring high quality, exceptional reliability, and outstanding moldability. USES: Passive electron.. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
Clariant Renol PA111G50 Nylon 66, 50% Glass Fiber Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D 790 |
BCC Products Proto-Kast BC 8163 Urethane Casting BC 8163 is a very low viscosity, rapid setting, rigid urethane compound. This system will cure quickly to a hard, tough, impact resistant casting. BC 8163 is non-sensitive to moisture after cure and.. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | Tangent; ASTM D790 |
Applied Composites 175 Vinylester SMC Industry Application: TransportationProduct Application: Structural ExteriorDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Flexural Modulus | 15.2 - 16.5 GPa | 2200 - 2400 ksi | |
Bulk Molding Compounds BMC 1410 Electrical Grade BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally.. |
|||
Flexural Modulus | 15.2 GPa | 2200 ksi | ASTM D790 |
PolyOne Edgetek® SF-45GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |