Mechanical Properties Metric English Comments
Flexural Modulus 0.152 GPa
22.0 ksi
ASTM D790
PolyOne Maxxam™ FR MF5420-0013 FR Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
Flexural Modulus 0.152 GPa
22.0 ksi
1% Secant; ASTM D882
M. Holland Company LD219AA LDPE  (discontinued **)
Features: Good Processability, Ultra High ToughnessUses: Bottles, PackagingProcessing Method: Blow MoldingInformation provided by M. Holland.
Flexural Modulus 0.152 GPa
22.0 ksi
1% Secant, Procedure A; ASTM D790
LyondellBasell Adflexâ„¢ Q 200 F Polyolefin
Description: Adflexâ„¢ Q 200 F fractional melt flow, low modulus thermoplastic olefin (TPO) resin is designed for extrusion applications. It is based on material produced from Basell's propri..
Flexural Modulus 0.152 GPa
22.0 ksi
3 pt. secant; ASTM D790
Chevron Phillips Marlex® 1122B Injection Molding Resin
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Excellent Flexibility, Moderate Flow, Moderate Warping Resistance, Moderate Mold Release, Excellent ESCRApplicati..
Flexural Modulus 0.152 GPa
22.0 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A
Dow FLEXOMER™ GRSN-1539 NT 7 Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ GRSN-1539 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins ..
Flexural Modulus 0.152 GPa
22.0 ksi
TD; ASTM D790
Diamond Polymers NPP10-0218 Low Density Polyethylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 0.152 GPa
22.0 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A
Dow FLEXOMER™ DFDA-1010 NT 7 Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDA-1010 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins ..
Flexural Modulus 0.152 - 2.21 GPa
22.0 - 320 ksi
Average value: 0.366 GPa Grade Count:18
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum ..
Flexural Modulus 0.152 GPa
22.0 ksi
ASTM D412
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Copyright © lookpolymers.com All Rights Reserved