Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.5 GPa @Temperature 23.9 °C |
2100 ksi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 120 E-Glass Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Quantum Composites QC-3450 48% Glass Fiber High Temperature Use SMC
(discontinued **) QC-3450 is highly reinforced with glass fibers. It is designed for compression molding of components requiring high structural strength and good resistance to elevated temperatures. Long-term use .. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Quantum Composites QC-7752 50% Glass Fiber Heat Resistant Polyester SMC
(discontinued **) QC-7752 is a modified polyester sheet molding compound (SMC) that is designed for applications requiring high strength, good environmental resistance, and resistance to elevated temperatures. It of.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 IM HS L 60% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ISO 178 |
Polyram Polytron P60B04-S Polypropylene, 60% Long Glass Fiber A chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.Information provided by Polyram. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 433 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
Asahi Kasei Thermylon® NSG-730A 65% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ISO Data |
BASF Ultramid® B3EG10 BK00564 50% Glass Filled PA6 (Dry) Ultramid B3EG10 BK00564 is a 50% glass fiber reinforced injection molding PA6 grade. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ASTM D790 |
PolyOne Gravi-Tech™ GRV-NY-060-CU Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Flexural Modulus | 14.5 GPa | 2100 ksi | ISO 178 |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |