Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 120 E-Glass Reinforced

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Park Electrochemical Corp.
Trade Name Nelcote®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 120 E-Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low Dk/Df values for demanding RF / microwave applicationsSelf adhesive bond to foam coresLong ambient out-time for easy processingEasily processed in both vacuum/oven and autoclave processesA cost effective, shop-friendly alternative to BMI and Cyanate Ester materials in many applicationsResistant to fungus, moisture, rain impact, and most chemicalsApplications/Qualifications:High performance radomesSignature control devicesUS Army HelicopterAir Force Ground-Based RadarInformation provided by Park Electrochemical Corp.
Physical Properties Metric English Comments
Volatiles <= 2.0 %
<br>@Temperature 288 °C
<= 2.0 %
<br>@Temperature 550 °F
10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 276 MPa
<br>@Temperature 23.9 °C
40000 psi
<br>@Temperature 75.0 °F
0° Direction, Dry; ASTM D638
Tensile Modulus 16.5 GPa
<br>@Temperature 23.9 °C
2400 ksi
<br>@Temperature 75.0 °F
0° Direction, Dry; ASTM D638
Flexural Strength 372 MPa
<br>@Temperature 23.9 °C
54000 psi
<br>@Temperature 75.0 °F
Dry; ASTM D790
Flexural Modulus 14.5 GPa
<br>@Temperature 23.9 °C
2100 ksi
<br>@Temperature 75.0 °F
Dry; ASTM D790
Compressive Strength 262 MPa
<br>@Temperature 23.9 °C
38000 psi
<br>@Temperature 75.0 °F
Dry; ASTM D695
Compressive Modulus 15.9 GPa
<br>@Temperature 23.9 °C
2300 ksi
<br>@Temperature 75.0 °F
Dry
Processing Properties Metric English Comments
Gel Time 1.00 - 1.50 min
<br>@Temperature 171 °C
1.00 - 1.50 min
<br>@Temperature 340 °F
Shelf Life 3.00 Month
<br>@Temperature 4.44 °C
3.00 Month
<br>@Temperature 40.0 °F
6.00 Month
<br>@Temperature -17.8 °C
6.00 Month
<br>@Temperature 0.000 °F
Descriptive Properties Value Comments
Prepreg Resin Content (%) 26-33
Resin Flow (%) 6-14
350°F, 100psi