Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.10 GPa | 160 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), 1 % Secant; ASTM D790 |
Network Polymers NPP 25-0216 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 50-1060 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.10 GPa @Temperature 23.0 °C |
160 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYelast TPE 10012 R3 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1% secant; ASTM D790A |
Reliance Industries Repol B550MN Polypropylene REPOL Polypropylene B550MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM200LN Polypropylene Impact Copolymer COPYLENE™ CM200LN has a superior balance of stiffness and impact strength. The high melt flow allows for quick filling of molds and the antistat and nucleation facilitates fast cycle times.Applicat.. |
|||
Flexural Modulus | 1.10 - 17.9 GPa | 160 - 2600 ksi | Average value: 7.09 GPa Grade Count:96 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Flexural Modulus | 1.10 - 113 GPa | 160 - 16300 ksi | Average value: 10.5 GPa Grade Count:272 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax 7823 Polypropylene Impact Copolymer, Fractional Melt Flow Key Features: high extrudate melt strength, good cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: pipe, tubing, sheet, profiles, netting, blown containers and i.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax SG702 Polypropylene Impact Copolymer Key Features: excellent cold impact resistance, good stiffness and impact balance, UV stabilizer, polypropylene copolymer resin, injection moldingApplications: automotive interior trim, pet carriers.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1% Tangent, 1.27 mm/min; ASTM D790A |
I. Stern 320NB Prime Impact Copolymer Polypropylene, No Break Features:Outstanding impact strength balanced with stiffnessExcellent long term heat aging propertiesWet/dry environment resistanceGood surface glossApplicationsAutomotiveApplianceLawn and GardenRig.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 2500H Polypropylene Block Copolymer CHARACTERISTICS: EXCELLENT HIGH IMPACT, HIGH TOUGHNESS GOOD EXTRUDABILITYAPPLICATIONS: SHEET / BLOW MOLD EXTRUSION AND INJECTION MOLDING FOR CORRUGATE SHEETS, SHEETS FOR FILE, HOUSEWARES, CONTAINERS.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn BA65H Polypropylene Copolymer, Flame Retardant Key Features: high melt flow, medium modulus, flame retardant polypropylene copolymer, good electrical properties, good aesthetics and colorability, good processabilityApplications: furniture, small.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn NXO-21001 Polypropylene Copolymer Key Features: high melt flow, medium modulus polypropylene copolymer, high flow, excellent processability, excellent colorabilityApplications: wire harnesses, housings, thin walled partsDescription:.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
LyondellBasell Hostacomâ„¢ BG749GC/1 Polypropylene Copolymer Description: Hostacomâ„¢ BG749GC/1 medium melt flow, 1,100 MPa flexural modulus, UV-stabilized, precolored, 20% calcium carbonate-filled polypropylene copolymer resin has an excellent combination.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7450 PP SABIC® PPcompound 7450 is a mineral filled, impact modified polypropylene TPO. This material can exhibit high impact resistance and good paintability in automotive exterior applications. The IMDS.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1% Secant; ASTM D790 |
Plastics Group Polifil® RP-HDPE High Density Polyethylene Polifil® RP-High Density Polyethylene is a moderate stiffness material that retains excellent toughness. HDPE exhibits outstanding chemical resistance and environmental stress crack resistance. Inj.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
Unipetrol PE HD LITEN® BB 85 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 504 Polypropylene Impact Copolymer Made for injection molding applications. Slip and antiblocking agent stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1.3 mm/min, tangent; ASTM D790 |
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | |
TriStar TriSteel PR Metal Backed PTFE Bearing System Ultraflon 602e enhanced PTFE (PR) lined metal backed bearing , high speed reciprocating, self lubricating, high temperature and high load applications. Liner is designed specifically for high freque.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 2% Secant; ASTM D790B |
ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
Eurostar Starflam M10009XP PP, Flame Retardant, Injection Molding Starflam M10009XP is an Unfilled Flame Retardant Polypropylene (Copolymer) Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Clariant Renol PA2SP0004 Nylon 6 Alloy Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | SAE J949 |
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | >= 1.10 GPa | >= 160 ksi | ASTM D790 |
Buckeye Polymers BP RPPC 1020 TU BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Carmel Olefins CAPILENE® SU 75 AV Polypropylene Impact Copolymer Description: CAPILENE® SU 75 AV is a high melt flow rate, controlled rheology impact copolymer for injection molding. CAPILENE® SU 75 AV is nucleated with antistatic additive. It offers outstand.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Buckeye Polymers BP Flex D8020 UC85 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PH 91 N Polypropylene Homopolymer FeaturesModified homopolymer PP for injection moulding. General use in all industry branches - packing material, garden flower-pots, toys, furniture industry, hinges, fasteners, clamps, office chai.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.10 - 6.40 GPa | 160 - 928 ksi | Average value: 2.01 GPa Grade Count:15 |
Overview of materials for Polypropylene with 10% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are .. |