Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.900 GPa | 131 ksi | |
Plastcom SLOVALEN PQ 83 N PP, imp. strength FeaturesPP modified with natural caoutchouc. The addition of thermoplastic caoutchouc causes increased toughness. General application in all industry branches. Delivered in natural mode and in the f.. |
|||
Flexural Modulus | 0.900 - 1.30 GPa | 131 - 189 ksi | |
Reliance Industries Polypropylene Random Copolymer Typical properties of Reliance - Repol Polypropylene gradesInformation provided by Reliance Industries |
|||
Flexural Modulus | >= 0.900 GPa | >= 131 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 6844G (446H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9326 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9646T HDPE High Molecular Weight Sheeting Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 4976 Classification: PE 235, A 56606Applications:Sheeting, Thermoforming, Profile ExtrusionData provided by Chevron Chemical. |
|||
Flexural Modulus | >= 0.900 GPa | >= 131 ksi | ASTM D790 |
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Iran Petrochemical (PCC) EP2C 37 F Polypropylene EP2S 37 F offers good process ability, excellent clarity and gloss and exhibits very good heat weld ability.Applications: packaging of stationery, packaging of food stuffs, lamination.Information pr.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Iran Petrochemical (PCC) EP2S 30 B Polypropylene This is a medium modified PP random copolymer. The product is designed for the extrusion of film and sheet and for blow molding small and medium sized item.Applications: Packaging of cosmetics, d.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5301 EA HDPE Blow Molding Applications:High performance blow molded containers typically of to 60 liters capacity for packaging aggressive productsRobust industrial and technical moldingsInformation provided by Interchim s.r.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H1000PBL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weathering, good balance of MRS and SCGRecommended Applications: Water pressure pipes and stripe lines for PE100 pi.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | at 70°C, tangent |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Borealis Borclear™ RE936CF Polypropylene Random Copolymer Borclear™ RE936CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: food packaging, lamination films, and stationary fil.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Unipetrol PE HD LITEN® LS 87 HDPE Made for special applicationsInformation provided by Unipetrol RPA |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Unipetrol PE HD LITEN® MB/ML 62 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Unipetrol PE HD LITEN® MB/ML 87 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 7001 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 179 |
Total PPM R021 Polypropylene, Random Copolymer for Medical Grade Polypropylene PPM R021 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D178 |
Total PPR 3221 Random Copolymer Polypropylene, Blow Molding and Sheet Extrusion Polypropylene PPR 3221 is a high clarity, high impact resistance random copolymer especially designed for blow molding applications (mono and multi-layers) for food and non-food packaging of sauces,.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | at 70°C, tangent |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Unitika A1030SR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
Tipco Tipcolene® TPE 1000 - Impact Modified Polypropylene Copolymer Compound with High Stiffness High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 2% Secant; ASTM D790 |
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin Resin Type: Hexene CopolymerCharacteristics: Good melt strengthExcellent ESCRApplications: ConduitDuctInformation provided by Chevron Phillips. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | cond; ISO 178 |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Flexural Modulus | >= 0.900 GPa | >= 131 ksi | ISO 178 |
AKG Polymers Vision PP PPC BL1008 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | SAE J949 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
Buckeye Polymers BP PPC 0412 R Blk Reprocessed Polypropylene, Unfilled BlackThis reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin compounds are ut.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
Carmel Olefins CAPILENE® QM 45 F Propylene Random Copolymer Description: CAPILENE® QM 45 F is a slip and anti-block formulated random copolymer. It is characterized by high gloss and easy processing.Applications: CAPILENE® QM 45 F is suitable for cast u.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
Asahi Glass Fluon® ETFE A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 2mm/min; ASTM D790 |
3M Dyneon™ PVDF 11010/0000 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 11010/0000 is a copolymer of VF2 and HFP (hexafluoropropylene). Recommended for flared tubing, it combines excellent chemical resistance, and dimensional stability with a moderate.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXFLEX® 980HF TPO
(discontinued **) Description: DEXFLEX® 980HF is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope.. |