Polymer Property : Flexural Modulus = 19.3 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.83 - 19.3 GPa
700 - 2800 ksi
Average value: 9.22 GPa Grade Count:21
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
Flexural Modulus 1.55 - 19.3 GPa
225 - 2800 ksi
Average value: 2.35 GPa Grade Count:214
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Flexural Modulus 0.103 - 19.3 GPa
14.9 - 2800 ksi
Average value: 5.43 GPa Grade Count:176
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Flexural Modulus 8.27 - 19.3 GPa
1200 - 2800 ksi
Average value: 14.8 GPa Grade Count:20
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Flexural Modulus 2.90 - 19.3 GPa
420 - 2800 ksi
Average value: 8.67 GPa Grade Count:46
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Flexural Modulus 17.2 - 19.3 GPa
2500 - 2800 ksi
Average value: 18.1 GPa Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% ..
Flexural Modulus 2.76 - 19.3 GPa
400 - 2800 ksi
Average value: 8.51 GPa Grade Count:18
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..