Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.03 GPa | 1310 ksi | ASTM D790 |
Niche Polymer PA66GF33BK Nylon 66, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 9.03 GPa | 1310 ksi | ASTM D790 |
Niche Polymer PA66GF33N Nylon 66, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 9.03 GPa @Thickness 3.17 mm |
1310 ksi @Thickness 0.125 in |
|
KEP Kepital® FG2025 25% Glass Fiber Reinforced Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 9.03 GPa | 1310 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY RF208 PA 66 LNP LUBRILOY* RF208 is a compound based on Nylon 66 resin containing 40% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 9.03 GPa | 1310 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY RF208 PA 66 (Asia Pacific) LNP LUBRILOY* RF208 is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 9.03 GPa | 1310 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp WC003P Polyester Elastomer LNP* Thermocomp* WC003P is a compound based on Polyester resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Flexural Modulus | 9.03 GPa | 1310 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QFL17RS PA 6/10 LNP LUBRICOMP* QFL17RS is a compound based on Nylon 6/10 resin containing 35% Glass Fiber, 5% PTFE. Added features of this material include: Easy Release, Heat Stabilized, Wear Resistant. |
|||
Flexural Modulus | 9.03 GPa | 1310 ksi | ISO 178 |
Polyplastics Duranex® 3300 Polybutylene Terephthalate (PBT), Standard, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 9.03 GPa | 1310 ksi | ASTM D790 |
LNP Thermocomp® JF-1006 BK8-115 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Flexural Modulus | 9.03 GPa | 1310 ksi | ASTM D790 |
LNP Lubricomp® QFL-4017 ER HS Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(discontinu Features: Heat Stabilized, Good Mold Release, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; .. |