Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.34 GPa | 1210 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXP PC LNP* Lubricomp* DFL36XXP is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | ASTM D790 |
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Flexural Modulus | 8.34 GPa @Thickness 6.40 mm |
1210 ksi @Thickness 0.252 in |
3mm/min; ASTM D790 |
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 8.34 GPa @Thickness 3.20 mm |
1210 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID SG2300B(W) PA66+GF30%, General Purpose, Good Surface Feature: Injection Molding, PA66+GF30%, General Purpose, Good SurfaceApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN332G30VO G/F Reinforced & Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | DIN 53452; ASTM D790 |
Kolon KOPET® KP133G30 FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | DIN 53452; ASTM D790 |
Kolon SPESIN® KP213G30 Flame Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Flexural Modulus | 8.34 GPa @Thickness 3.20 mm |
1210 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2306FB PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 8.34 GPa @Thickness 3.20 mm |
1210 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 8.34 GPa @Thickness 3.20 mm |
1210 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2306FI PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical.. |
|||
Flexural Modulus | 8.34 GPa @Thickness 3.20 mm |
1210 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
Flexural Modulus | 8.34 GPa @Thickness 3.20 mm |
1210 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® NH2306F PBT+GF30% Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | ASTM D570 |
LG Chemical Lupox® PBT-GP-2306F 30% GFR Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | 5 mm/min; ISO 178 |
Gromax BFG30-FH00B2 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | ASTM D790 |
Gromax PBT 3030-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | ASTM D790 |
Gromax PBT 4130-104D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 8.34 GPa @Thickness 3.20 mm |
1210 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2306FG PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | 5 mm/min; ISO 178 |
Gromax BFG30-FH00B1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX5558 PPE+PS 30% glass reinforced, high flow PPO. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | |
Shinil Chemical SHINFLAME PA-66 GF Flame Retardant Polymer Under Hood SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | |
Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite CHC SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | ASTM D790 |
Techmer Lehvoss Compounds Luvotech™ J-4/30 BK PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | ASTM D790 |
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 BK2989 PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | ASTM D790 |
Techmer Lehvoss Compounds Luvotech™ J-4/35 BK223 PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | ASTM D790 |
Techmer Lehvoss Compounds Luvotech™ J-4/35 NAT PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Flexural Modulus | 8.34 GPa | 1210 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PH0800A PA 6 LNP* THERMOCOMP* PH0800A is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity. |