Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.40 GPa | 928 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 SGF 30 Polyamide 6, 30% Milled Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% of milled glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consum.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Nilit FRIANYL A63 HS-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | <= 6.40 GPa | <= 928 ksi | |
Reliance Industries Polypropylene - 30% glass fiber filled Information provided by Reliance Industries |
|||
Flexural Modulus | <= 6.40 GPa | <= 928 ksi | |
Reliance Industries Polypropylene - Suzorite mica (untreated) filler Information provided by Reliance Industries |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
Shell Carilon® DB6F5G40 Polyketone, Flame-Retarded (V-0), 20% Glass-Reinforced Injection Molding Grade
(disco Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F5G40 is a flame-retarded, 20 percent glass-fiber-reinforced, injection molding grade with mecha.. |
|||
Flexural Modulus | 6.40 GPa @Temperature 23.0 °C |
928 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B22^ E F20 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 6.40 GPa @Temperature 60.0 °C |
928 ksi @Temperature 140 °F |
ASTM D790 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
LG Chemical LUCEL CF-610 Electrically Conductive POM, 10% Carbon Fiber Filled, High Strength, Wear Resistant LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
LG Chemical Lupox® HI-2302 High Impact PBT, 30% Glass Fiber Reinforced LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178-A |
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178-A |
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP (Europe-Africa-Middle East) LNP* Lubricomp* MFL36S is a compound based on Polypropylene resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66 LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, Conditioned Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, DRY Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
Plenco 7100 Phenolic, Nodular, Injection Molded PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Polyplastics FR-PET® BN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Polyplastics FR-PET® CN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ISO 178 |
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
Ashley Polymers Ashlene® 527LD-33G Nylon 66, High Impact, 33% Glass Reinforced A high impact reinforced Nylon 66 with good low temperature properties.Data provided by the manufacturer |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
Chem Polymer Chemlon 225 G Nylon 6, 25% Glass Fiber Reinforced A 25% glass fiber reinforced nylon 6 offering a balance of properties between the 20% (Chemlon 220 G) and 30% (Chemlon 233 G) product offerings. This product offers further improvements in tensile .. |
|||
Flexural Modulus | 6.40 GPa | 928 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 272 Polystyrene Alloy, Glass Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |