Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.00 GPa | 725 ksi | |
Plastcom SLOVAMID 66 GF 15 HI PA66, 15% glass fibre FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Flexural Modulus | 5.00 GPa @Temperature 23.0 °C |
725 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYabs N20 GF17 ABS, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ASTM D790 |
NHEP Spectron™ E6126 Nylon 66, 20% Glass Fiber Natural color. E6126 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati.. |
|||
Flexural Modulus | 5.00 GPa @Temperature 90.0 °C |
725 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim.. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ISO 178 |
Nilit FRIANYL A63 CV-CM 0830 9005/Z Powder-coatable nylon 6.6 for injection molding, 8% carbon fiber reinforced, 30% ceramic filled Powder-coatable nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.00 GPa @Temperature 23.0 °C |
725 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A12^ Q40 Nylon 66, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | Transverse |
Quadrant Plastic Composites MultiQ® Impact Thermoplastic Panel Composite MultiQ is a product line of thermoplastic composites in panel form whose specific properties make them particularly suitable as an environmental alternative to plywood in outdoor applications. Howev.. |
|||
Flexural Modulus | 5.00 - 10.0 GPa | 725 - 1450 ksi | ASTM D790 |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Flexural Modulus | 5.00 GPa @Temperature 23.0 °C |
725 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH MGF5040 Polypropylene Homopolymer, Multifiller Information provided by Polykemi AB |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ISO 178 |
Nilit FRIANYL B63 SG-GV 2010 Nylon 6 for injection molding, 20% mineral filled and 10% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.00 - 17.3 GPa | 725 - 2510 ksi | Average value: 10.0 GPa Grade Count:72 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Flexural Modulus | 5.00 - 25.5 GPa @Temperature -40.0 - 250 °C |
725 - 3700 ksi @Temperature -40.0 - 482 °F |
Average value: 13.8 GPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN333G15 G/F Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | |
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR/BK Polyether sulfone, with glass fiber, easy flowing, demolding aid Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ASTM D790 |
Samyang Tribit® 1500A15 PBT, Inorganic Reinforced Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500A15 contains inorganic filler.Applicati.. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF003AS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF003AS is a compound based on Polyphthlamide resin containing Glass Fiber. Added features include; Heat Stabilized. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ASTM-D790 |
Polyram PlusTek PB300G3 Nylon 6, 15% Glass Fiber 15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ASTM-D790 |
Polyram PlusTek PB305G33 Nylon 6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized and UV stabilized polyamide 6 approved and listed by W.R.C and NSF/ANSI 61 international for potable waterInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | Tangent; ASTM D790 |
Washington Penn H2GF3 Polypropylene, 30% Glass Fiber Reinforced Homopolymer. Excellent heat aged physical properties.Applications: Under hood applications, battery trays, exercise equipmentData provided by Washington Penn Plastic Co., Inc. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ISO 178 |
Wellman Wellamid® GF13-66 22LH-N 13% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ASTM-D790 |
Polyram RamShine PV300G4 ABS, 20% Glass Fiber 20% glass fiber reinforced, heat resistant and minimal mold shrinkage ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | D790 |
Zhejiang Juner 301-G15 15% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Flexural Modulus | >= 5.00 GPa | >= 725 ksi | ASTM-D790 |
Polyram PlusTek RA300G4 Nylon 6.6, 20% Glass Fiber 20% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ASTM D 790 |
Cossa Polimeri ESTADIENE 0417 GIF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | from bending test; DIN 53 457 |
Hippe PAI Polyamide-imide Particularly used where high strength in a wide range of temperature (-190°C…+260°C), high notched strength and very good dielectric properties are required. Features good chemical stability, fl.. |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ISO 178 |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned) Information provided by BASF |
|||
Flexural Modulus | 5.00 GPa | 725 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 431 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 5.00 - 8.00 GPa | 725 - 1160 ksi | ISO 178 |
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati.. |
|||
Flexural Modulus | 5.00 - 27.6 GPa | 725 - 4000 ksi | Average value: 11.8 GPa Grade Count:38 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |