Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.10 GPa | 450 ksi | |
Plastcom SLOVALEN PH 66 GF 20 FRO 4 PP, 20% glass fibre, flame retardant FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, with decreased flammability. Used in the electrical industry - teroderately increased toughness an.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
PolyOne Nymax™ 604 NU Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Flexural Modulus | 3.10 GPa @Temperature 90.0 °C |
450 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Polymer Resources NY66-GP1 General Purpose Nylon 66 General Purpose Nylon 66, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Flexural Modulus | 3.10 GPa @Temperature 23.0 °C |
450 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
PolyOne Lubri-Tech™ NL-15KV/05M Nylon 6/12 - 15% Kevlar Fiber - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Global PEI-110 Easy Flow, Polyetherimide Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
Lucite International Diakon® Frost 902 70 Acrylic Polymer Information provided by Lucite International |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | |
Ineos Styrenics Polystyrene 148G (NAFTA) High heat, easy flow general purpose polystyrene with excellent clarity. Designed for applications requiring a combination of fast processing with good strength and heat resistance.Information prov.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM AUT195 PEI+PCE High flow Polyetherimide blend for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 195C (SABIC test method). |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Styrolution PS-148G Polystyrene Description: Polystyrene 148G is a high heat, easy flow general purpose polystyrene with excellent moldability, clarity and fast set-up time. It can be utilized as a coextruded gloss cap over high i.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Techmer ES Electrablend® ABS SS7 MB 7% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Techmer ES Luriblend® HTN 01410 BK Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant and Molybdenum Disulfide LubricantFeatures: Good Wear Resistance, Low Friction, High Heat Resistance and LubricatedAppear.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |