Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP CMX8030 VT Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF1020 Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific) LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | |
Lehmann & Voss LUVOCOM® 1105-8059 PEEK, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | |
Lehmann & Voss LUVOCOM® 1301-8349 PPS, linear, with PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage .. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ASTM D790 |
Mitsui Arlen™ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178 |
Lucite International Diakon® LG702 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178 |
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | |
Lehmann & Voss LUVOCOM® 1-7830 Polyamide 66, with PTFE, lubricant modified, improved wear resistance, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | |
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Europe-Africa-Middle East) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific) LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178-93 |
Wellman Wellamid® FR1841-BK1 Nylon 66, Unfilled, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178-93 |
Wellman Wellamid® GS1791-N2 5% Glass Sphere Reinforced, Natural Nylon 66 Description: Glass Sphere Reinforced, Natural Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ASTM D790 |
Cresset Powers Cress-Alon™ A3000 3.0 r.v. Film or Extrusion Grade Nylon 6, Dry As Molded Neat resin, for film or extrusion.Information provided by Cresset Powers Ltd. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178 |
Eurostar Starpylen HU 30BF4 PP, 30% Bamboo Fiber Filled, Injection Molding Starpylen HU30BF4 is a 30% Bamboo Fiber Reinforced Polypropylene Injection Molding Resin (also known as HU30BF4) (PRELIMINARY DATASHEET)Information provided by Eurostar. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 100KM NC000 Acetal (POM)
(Unverified Data**) Kevlar® Modified High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100KM is a high viscosity acetal homopolymer resin modified with Kevlar aramid resin. It is designed for appl.. |
|||
Flexural Modulus | >= 3.00 GPa | >= 435 ksi | ISO 178 |
AKG Polymers Vision PP PPH BL1303 G30 Polypropylene Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ISO 178 |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Flexural Modulus | 3.00 GPa | 435 ksi | ASTM D790 |
Chem Polymer Formax 605 G Acetal, 5% Glass Reinforced A lubricated, 5% glass reinforced acetal offering a balance of rigidity, dimensional stability and tensile strength.Data provided by the manufacturer, Chem Polymer. |