Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87416 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
PolyOne LubriOne™ NN-000/15T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | Tangent; ASTM D790 |
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | Tangent; ASTM D790 |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E7364 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | Tangent; ASTM D790 |
RheTech Products M25P100-01 25% Mica Reinforced Polypropylene, Black Applications: Underhood applicationsInternal I/P ComponentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
LNP Lubricomp® LL-4040 Polyetheretherketone, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.96 GPa @Thickness 3.18 mm, Temperature 23.0 °C |
429 ksi @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D790 |
PolyOne Geon™ Vinyl Fittings M1015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK LNP* LUBRICOMP* LL004C is a compound based on Polyetheretherketone resin containing 20% PTFE. Added features of this material include: Wear Resistant, Clean Compounding System. |
|||
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing Aramid, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 LNP* LUBRICOMP* RAL22S is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 (Asia Pacific) LNP* Lubricomp* RAL22S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Techmer ES Luriblend® POM HO TL2 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(2%)Features: Lubricated, Good Wear Resistance and HomopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KB003RXZ Acetal Copolymer LNP THERMOCOMP* KB003RXZ is a compound based on Acetal Copolymer resin containing 15% Glass Bead. Added features of this material include: Easy Release. |
|||
Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Total PSC 536 Polystyrene Polystyrene 536 is a high melt flow; high heat crystal polystyrene. Designed for fast cycle injection molding and for high output, direct injection profile extrusion for foam applications.Informatio.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
Total PSC 585 Polystyrene Polystyrene 585 is a high molecular weight, low melt flow, crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. 585 also mak.. |
|||
Flexural Modulus | 2.96 GPa @Temperature 22.8 °C |
430 ksi @Temperature 73.0 °F |
ASTM D790 |
Ensinger TECAPET™ PET Polyethylene Terephthalate (PET) TECAPET™ PET is an unreinforced, semicrystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus,.. |
|||
Flexural Modulus | 2.96 - 13.4 GPa | 430 - 1950 ksi | Average value: 8.50 GPa Grade Count:13 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D-790 |
Axiall 3101 Rigid PVC, Extrusion Georgia Gulf 3101 is a powder blend designed for the extrusion of window, door and fence profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia Gulf be.. |