Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2320 LCW Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Oxford Polymers Polysulfone PSF P170-64170 White PSU Product Description: Polysulfone injection molding grade, precolored white Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Continuous use up to 300(f)Informatio.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
PTS Trimid® N66-100L Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Fittings 211 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
PolyOne LubriOne™ ATH-000/05T Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ISO 178 |
Ravago Manufacturing Americas Hylon® N1200HL BK Nylon 6/6
(discontinued **) Available in North AmericaAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedAuto Specifications: DELPHI QMPL-1257 Color: BlackForm: PelletsInformation provided by Rava.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
BASF Capron® 8202 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 E U Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: ExtrusionTPCI# 9777102Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 E40 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF/M15 A1 BK 15% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 15% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized Appearance: BlackInformation provided by TP Compo.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 HS L BK Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: BlackTPCI# 7190102Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 HS L Colors Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: Colors AvailableTPCI# 10014102Information provided by TP Composite.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 HS YL030 Heat Stabilized Availability: North AmericaForms: PelletsFeatures: Fast Molding Cycle and Good AdhesionAppearance: YellowTPCI# 10054102Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 L N MB (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability and NucleatedTPCI# 7964102Information provided by TP Co.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 L N YL038MB Availability: North AmericaForms: PelletsAdditive: Lubricant, UV Stabilizer and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Good UV Resistance and NucleatedAppeara.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 L UV (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES Luriblend® PA6 E ML2 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MFB22S PP LNP* THERMOCOMP* MFB22S is a compound based on Polypropylene containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Heat Stabilized. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 HS L Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedTPCI# 7190102Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
PlastxWorld CEVIAN® CGF10 10% GF PC/Acrylic Alloy Glass fiber reinforced PC/Acrylic alloy.These are typical values and are not intended for specification purposes. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN300HL (Dry) Nylon 66, Heat Stabilized, Lubricated Features: General purposeHeat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Clariant Renol PA112 Nylon 66, Nucleated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Clariant Renol PA111BK S&P Nylon 66, General Purpose Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | JIS-K-6740 |
Denka VINYKON R3102 PVC, R grade for hard extrusion A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Flexural Modulus | 2.83 - 7.60 GPa | 410 - 1100 ksi | Average value: 4.61 GPa Grade Count:25 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |