Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.82 GPa | 409 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
Flexural Modulus | 2.82 GPa @Thickness 3.20 mm |
410 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® GP1000A PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl TN240 PPE+PS PPE+PS blend. Unfilled. Transparent. Good flow. Scratch resistant. Injection molding. Suitable for housewares, personal care and small appliance applications.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl TN240 PPE+PS (Asia Pacific) PPE+PS. Transparent. High flow, scratch resistant. Injection molding. Housewares and small appliances applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL TN300 PPE+PS PPE+PS. Transparent. High heat. Color Limited. Injection molding. Laser-Transmission welding applications. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66 LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubriloy D20001 PC LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.This data was supplied by.. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific) LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009 PC LNP* STAT-KON* DD0009 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Asia Pacific) LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009 PC (Europe-Africa-Middle East) LNP* Stat-kon* DD0009 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing, Flame Retardant... |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009P PC (Asia Pacific) LNP STAT-KON* DD0009P is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Europe-Africa-Middle East) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC (Asia Pacific) LNP* Stat-kon* DD0009XP is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include:Electrically Conductive, Flame Retardant. Also known as Stat-Kon*.. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX03571 PC LNP* STAT-KON* DX03571 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX03571 PC LNP* STAT-KON* DX03571 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP LNP* THERMOCOMP* MX88028 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
Teknor Apex APEX® RM 8216 Polyvinyl Chloride, Rigid Forms: PelletsInformation Provided by Teknor Apex |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP (Asia Pacific) LNP* Thermocomp* MX88028 is a compound based on Polypropylene resin containing Glass Fiber. |
|||
Flexural Modulus | 2.82 GPa | 409 ksi | ASTM D-790 |
Axiall LSS-8200 Rigid PVC, Extrusion Georgia Gulf LSS-8200 is a special purpose rigid PVC sheet extrusion compound designated for reduced smoke emission properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |