Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.72 GPa | 395 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2020 LO-GC Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® 2020 LO-GC is a glass clear pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® FR23 ABS Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | ASTM D790 |
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS (Asia Pacific) 5% PTFE reinforced PC+ABS wear resistant flame retardant resin for moving components in business equipment. Medium heat performance |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C2805 PC+ABS LNP* Lubricomp* Cycoloy* C2805 compound is a PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY XTPMFR10 ASA+PC (Asia Pacific) Improved ASA/PC blend for high flow, 1.0mm V0 applications. Improved UV performance aesthetically and physically compared to alternatives. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS (Europe-Africa-Middle East) LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS wear resistant flame retardant resin for moving components in business equipment. Medium heat performance |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC LNP STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Clean Compounding System. Easy Molding, Electrically Conductive. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC (Asia Pacific) LNP* STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX04462C PC LNP STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | ASTM D790 |
Techmer ES Luriblend® POM CO TX10 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%) and LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX04462C PC (Asia Pacific) LNP* STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | ASTM D790 |
Teknor Apex Synres® PP G15 18 Polypropylene, Glass Reinforced Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many .. |
|||
Flexural Modulus | 2.72 GPa | 395 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801R PC+ABS LNP* Lubricomp* Cycoloy_C2801R compound is a 5% PTFE reinforced PC+ABS wear resistant, flame retardant compound for moving components in business equipment. 30% recycle content. |