Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.17 GPa | 315 ksi | Tangent; ASTM D790 |
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
PolyOne Trilliant™ HC X HC5200-0026 RS Natural Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Flexural Modulus | >= 2.17 GPa | >= 315 ksi | ASTM D790 |
S&E Specialty Polymers GPP1001HFNH-2-AT(18) PP Application: Non-halogen flame retardant UL-94 V0 polypropylene compound.Information provided by S&E Specialty Polymers |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific) ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EM3110R PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are.. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
PolyOne Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
Polymer Resources PC/TP-GP1 PC Polyester, High Impact, Good Chemical Resistance
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
Ineos Nova Zylar® 220 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarity Good elongation Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class VI plasticsApplications:D.. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | 0.05 in/min; ASTM D790 |
Ineos Nova Zylar® 220 High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent moldability, High clarity, Extended toughness and elongation, meets USP XXI specification for Class VI Plastics, Property retention after gamma irradiationApplications: Display, medical de.. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
Samsung Cheil Industries Starex® SD-0150 ABS, Unreinforced
(discontinued **) Amorphous Acrylonitrile Butadiene Styrene (ABS)Characteristics: General Purpose: Good Impact Strength, Chemical Resistance, ProcessabilityApplications: Household Appliances, Auto Interior Trim and P.. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP AL004 ABS LNP* Lubricomp* AL004 is a compound based on Acrylonitrile Butadiene Styrene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
Hannam Chemical Hanalac HFA-700 ABS |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific) LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | Type I, 1.3 mm/min; ASTM D790 |
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp WH0500B PBT LNP* THERMOCOMP* WH0500B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was .. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp WH0500B PBT (Asia Pacific) LNP* THERMOCOMP* WH0500B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was .. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
Chase Plastics CP Pryme® N310GL (COND, 50% RH) Nylon 6 (Utility Grade), 10% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® RMT-20 20% Talc-Reinforced Polypropylene, High Impact Polifil® RMT series compounds are high impact polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and high heat deflection resis.. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 7602B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D-790 |
Axiall 9246 Rigid PVC, Molding Georgia Gulf 9246 is a high impact compound suitable for food packaging.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
Adell YS-10 PC Alloy |
|||
Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
Ineos Nova 6100 Super High Impact Polystyrene
(discontinued **) Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen.. |