| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 7.5 g/10 min | 7.5 g/10 min | ASTM D1238G |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 102 | 102 | ASTM D785 |
| Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
| Elongation at Break | 40 % | 40 % | ASTM D638 |
| Flexural Yield Strength | 59.0 MPa | 8560 psi | ASTM D790 |
| Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
| Izod Impact, Notched | 1.20 J/cm @Thickness 3.17 mm |
2.25 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 77.0 °C | 171 °F | Heat Distortion Temp |
| Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648 |
| Vicat Softening Point | 42.0 °C | 108 °F | ASTM D1525 |
| Flammability, UL94 | V-0 | V-0 |