Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.5 GPa | 2390 ksi | ASTM D790 |
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr.. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ISO 178 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | |
Lehmann & Voss LUVOCOM® 50-7807 Polycarbonate, with carbon fiber and demolding aid Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | |
MTI ThermoStran® PP-30C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES Electrafil® J-1305/CF/20 PPS |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 CF30 30% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES Luriblend® PA4/6 CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance and Low FrictionInformation p.. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI LNP THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific) LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF50 FR BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 16.5 GPa | 2390 ksi | ISO 178 |
Polyram Polytron A50B01 Nylon 6.6, 50% Long Fiber Glass 50% Long fiber glass reinforced black Nylon 6.6, heat stabilized for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF50 FR UV X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightAdditive: Flame Retardant and UV StabilizerFeatures: Flame RetardantAppearance: BlackProcessing Method.. |
|||
Flexural Modulus | 16.5 GPa | 2400 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF50 FR-N BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 50% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc... |
|||
Flexural Modulus | 16.5 GPa @Temperature 23.0 °C |
2390 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |