Mechanical Properties Metric English Comments
Flexural Modulus 15.1 GPa
2190 ksi
(102 mm Span) 3mm/min; ASTM D790
LNP ULTEM® UC3000 Polyetherimide, 30% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..
Flexural Modulus 15.1 GPa
2190 ksi
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS.
Flexural Modulus 15.1 GPa
2190 ksi
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621..
Flexural Modulus 15.1 GPa
2190 ksi
ASTM D790
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy
Epiall 1908-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation proper-ties that meets the requir..
Flexural Modulus 15.1 GPa
2190 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East)
LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Flexural Modulus 15.1 GPa
2190 ksi
ASTM D790
Plenco 6015 Phenolic, Briquette, Transfer Molded
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf..
Flexural Modulus 15.1 GPa
2190 ksi
2 mm/min; ISO 178
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded
Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar.
Flexural Modulus 15.1 GPa
2190 ksi
ASTM D790
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr..
Flexural Modulus 15.1 GPa
2190 ksi
ASTM D790
Quantum Composites QC-8151C 55% Glass Fiber Vinyl Ester Static-Dissipative SMC  (discontinued **)
QC-8151C is a vinyl ester sheet molding compound (SMC) designed for compression molding components requiring dimensional stability, resistance to high temperatures plus sufficient electrical conduct..
Flexural Modulus 15.1 GPa
2190 ksi
(102 mm Span) 3mm/min; ASTM D790
LNP ULTEM® SMU5836 Polyetherimide, 30% Carbon Fiber Reinforcement  (discontinued **)
High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo..
Copyright © lookpolymers.com All Rights Reserved