Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quantum Composites QC-8151C 55% Glass Fiber Vinyl Ester Static-Dissipative SMC  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Vinyl Ester , Vinyl Ester Sheet Molding Compound
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quantum Composites QC-8151C 55% Glass Fiber Vinyl Ester Static-Dissipative SMC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QC-8151C is a vinyl ester sheet molding compound (SMC) designed for compression molding components requiring dimensional stability, resistance to high temperatures plus sufficient electrical conductivity to dissipate static charge. It also offers excellent chemical resistance, light weight, low heat absorption and high strength at both room and elevated temperatures. This electrical conductivity is built into and throughout the composite. It is designed to mold and cure at lower temperatures than QC-8150C. Form and Color = Rolled Sheet, Gray. Glass Fiber Length = 1 inch.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 206 MPa
29900 psi
ASTM D638
Flexural Yield Strength 344 MPa
49900 psi
ASTM D790
Flexural Modulus 15.1 GPa
2190 ksi
ASTM D790
Izod Impact, Notched 12.8 J/cm
24.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Shrinkage 0.00020 %
0.00020 %
Processing Properties Metric English Comments
Processing Temperature 93.0 - 121 °C
199 - 250 °F
Mold temperature
Copyright © lookpolymers.com All Rights Reserved