Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging VEO-111 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM003 Polypropylene Impact Copolymer CM003 is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes.Applications: Extrusion ProcessesInformation provided .. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | 1% Secant; ASTM D790 |
Flint Hills P4C5B-030 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Nucleated, antistat, and controlled rheology.Applications: Injection molding: closures and excellent mold release.Former Huntsman polypropylene.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific) LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | 1% Secant; ASTM D790 |
Washington Penn Homopolymer Polypropylene Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array .. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® 9514H Polyethylene; HDPE High density polyethylene. This gas phase, high molecular weight hexene copolymer is tailored for lightweight blow molded applications that: Require excellent stiffness to ESCR ratioRequire good m.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | Chord 0.39 in/min; ISO 178 |
ExxonMobil Exxtral™ CNT 001W Performance Polyolefin Product Description: High impact, medium melt flow rate copolymer, colored black. Particularly suitable for injection molded automotive interior & exterior applications. Availability: North America .. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow DMDA-8007 NT 7 High Density Polyethylene Resin DOW DMDA-8007 NT is a narrow molecular weight distribution high density homopolymer designed to offer excellent stiffness, low warpage, good/acceptable toughness, and good mold-ability. This resin .. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4040WT Impact Copolymer Polypropylene Description: Superior drop impact at refrigeration temperature, very high flexural modulus, nucleated, good mold release.Applications: Suggested uses include thermoforming, food packaging, dairy con.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4450M Impact Copolymer Polypropylene Description: Very High Flexural ModulusApplications: Suggested Uses Include Compounding, Automotive Interior Trim, Intricately Designed Parts, Thin-Walled Parts.Process: Compounding.This resin meets.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D-790 |
Bapolene® 4062 Polypropylene, Injection Grade Bapolene PP4062 is a high flow general purpose injection molding resin. This product meets FDA standards for food contact applications.Applications: Housewares, closures, spray caps, food containers.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
Chevron Phillips Marlex® HMN 5580 Polyethylene, Injection Molding Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520. High stiffness, excellent surface appearance, good impact strength and warpage resistance.Data provided by the manufacturer |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
Chevron Phillips Marlex® B592 Polyethylene, Injection Molding Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | Tangent; ASTM D790 |
Chevron Phillips Marlex® 9515H High Density Polyethylene, Blow Molding This gas phase, high molecular weight, hexane copolymer with antistatic agent is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt str.. |
|||
Flexural Modulus | 1.41 GPa | 205 ksi | Tangent; ASTM D790 |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |