Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
Manufacturer | PolyOne Corporation |
Trade Name | Geon™ |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | PolyOne Geon™ Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.33 g/cc | 1.33 g/cc | ASTM D792 |
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 83 | 83 | ASTM D2240 |
Tensile Strength, Yield | 52.4 MPa | 7600 psi | Type I, 5.1 mm/min; ASTM D638 |
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Flexural Modulus | 1.41 GPa | 205 ksi | ASTM D790 |
Izod Impact, Notched | 10.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.7 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Transmission, Visible | 82 % @Thickness 0.851 mm, Wavelength 700 nm |
82 % @Thickness 0.0335 in, Wavelength 700 nm |
Internal Method |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 193 - 210 °C | 379 - 410 °F | Blow Molding |
Descriptive Properties | Value | Comments |
---|---|---|
Appearance | Clear/Transparent | |
Features | General Purpose | |
High Gloss | ||
Medium Impact Resistance | ||
Forms | Pellets | |
Generic Material | PVC, Rigid | |
Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
Processing Method | Profile Extrusion | |
Regional Availability | Africa & Middle East | |
Asia Pacific | ||
Europe | ||
North America | ||
South America | ||
Uses | General Purpose | |
Packaging |