Mechanical Properties Metric English Comments
Flexural Modulus 0.305 GPa

@Temperature 120 °C
44.2 ksi

@Temperature 248 °F
ASTM D790
BASF Capron® 8200 NL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Modulus 0.305 GPa

@Temperature 120 °C
44.2 ksi

@Temperature 248 °F
ASTM D790
BASF Capron® 8202 NL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Modulus 0.305 GPa

@Temperature 120 °C
44.2 ksi

@Temperature 248 °F
ASTM D790
BASF Capron® 8224 HSL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Flexural Modulus 0.305 GPa
44.2 ksi
ASTM D790
Sumitomo Chemical ESPOLEX® WT515 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Flexural Modulus 0.305 GPa

@Temperature 120 °C
44.2 ksi

@Temperature 248 °F
ASTM Test
BASF Ultramid® 8202 HS PA6 (Dry)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
Flexural Modulus 0.305 GPa

@Temperature 120 °C
44.2 ksi

@Temperature 248 °F
ASTM Test
BASF Ultramid® 8202 PA6 (Dry)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
Flexural Modulus 0.305 - 5.50 GPa

@Temperature -40.0 - 120 °C
44.2 - 798 ksi

@Temperature -40.0 - 248 °F
Average value: 1.40 GPa Grade Count:8