Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.152 GPa | 22.0 ksi | ASTM D790 |
PolyOne Maxxam™ FR MF5420-0013 FR Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | 0.152 GPa | 22.0 ksi | 1% Secant; ASTM D882 |
M. Holland Company LD219AA LDPE
(discontinued **) Features: Good Processability, Ultra High ToughnessUses: Bottles, PackagingProcessing Method: Blow MoldingInformation provided by M. Holland. |
|||
Flexural Modulus | 0.152 GPa | 22.0 ksi | 1% Secant, Procedure A; ASTM D790 |
LyondellBasell Adflexâ„¢ Q 200 F Polyolefin Description: Adflexâ„¢ Q 200 F fractional melt flow, low modulus thermoplastic olefin (TPO) resin is designed for extrusion applications. It is based on material produced from Basell's propri.. |
|||
Flexural Modulus | 0.152 GPa | 22.0 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips Marlex® 1122B Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Excellent Flexibility, Moderate Flow, Moderate Warping Resistance, Moderate Mold Release, Excellent ESCRApplicati.. |
|||
Flexural Modulus | 0.152 GPa | 22.0 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A |
Dow FLEXOMER™ GRSN-1539 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ GRSN-1539 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins .. |
|||
Flexural Modulus | 0.152 GPa | 22.0 ksi | TD; ASTM D790 |
Diamond Polymers NPP10-0218 Low Density Polyethylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 0.152 GPa | 22.0 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 A |
Dow FLEXOMER™ DFDA-1010 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1010 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins .. |
|||
Flexural Modulus | 0.152 - 2.21 GPa | 22.0 - 320 ksi | Average value: 0.366 GPa Grade Count:18 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Flexural Modulus | 0.152 GPa | 22.0 ksi | ASTM D412 |
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |