Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0600 GPa | 8.70 ksi | Secant 1%; ASTM D-790-95 |
Multibase Multi-Flex® TPO 4107 BLK Data provided by Multibase. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | ISO 178 |
Polimeri Europa Clearflex® MP D0 Very Low Density Polyethylene Clearflex MP D0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | ISO 178 |
Polimeri Europa Greenflex® ML 40 Ethylene Vinyl Acetate Copolymer - Injection Molding Greenflex ML 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding of flexible items. Items produced with Greenflex ML 40 show high elasticity and flexibility.Main Applications: Gr.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | ASTM D790 |
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | ISO 178 |
Huntsman AVALON® 650 B Thermoplastic Polyurethane Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCD855 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SPE and NISPE confiations. Flame retardant performance capable of m.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON TX06488NTX1 PU LNP* STAT-KON* TX06488NTX1 is a compound based on Polyurethane resin containing Proprietary Filler(s). Added features of this grade are: Execllent Ductility, Electrically Conductive. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | ISO 178 |
Chengdu Polyster CH4132 Thermoplastic Polyether-ester Elastomer (TPEE) Poly-basic block copolymer. Good compatibility with POM. For blending with POM to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | ISO 178 |
Chengdu Polyster H4040 Thermoplastic Polyether-ester Elastomer (TPEE) Low modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent flex resistance, especially at low temperatures. Moldable even in thin sections. Can be used in light.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | 1% secant; ASTM D790 |
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | ASTM D638 |
Arkema Group LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3410 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3410 is a versatile adhesive for extrusion coating or lam.. |
|||
Flexural Modulus | 0.0600 GPa | 8.70 ksi | ASTM D638 |
Arkema Group LOTRYL® 16 MA 003 Copolymer Ethylene - Methyl Acrylate LOTRYL® 16 MA 003 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 16 MA 003 is a polymer o.. |