Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D-5420 |
Network Polymers NPP 808 C2WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Network Polymers NPP 808 C2WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -18.0 °C |
>= 26.7 ft-lb @Temperature -0.400 °F |
ASTM D5420 |
Network Polymers NPP 808 C3WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D-5420 |
Network Polymers NPP 808 C3WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Network Polymers NPP 808 C3WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -18.0 °C |
>= 26.7 ft-lb @Temperature -0.400 °F |
ASTM D5420 |
Network Polymers NPP 808 C4WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D-5420 |
Network Polymers NPP 808 C4WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -18.0 °C |
>= 26.7 ft-lb @Temperature -0.400 °F |
ASTM D5420 |
Network Polymers NPP 808 C5WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Network Polymers NPP 808 C5WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D-5420 |
Network Polymers NPP 808 C8 WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Network Polymers NPP 808 C8 WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -18.0 °C |
>= 26.7 ft-lb @Temperature -0.400 °F |
ASTM D5420 |
Network Polymers NPP 908 Description: Polyester CopolymerInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D-5420 |
Network Polymers NPP 908 Description: Polyester CopolymerInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420-96 |
LyondellBasell SEQUEL® E3000 FR TPO Description: SEQUEL® E3000FR thermoplastic olefinic elastomer (TPO) is designed for exterior and interior applications that require stiffness and durability. This extrusion-grade material is spe.. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420-96 |
LyondellBasell SEQUEL® E3000 TPO Description: SEQUEL® E3000 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require toughness and dimensional stability. This extrusion.. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Diamond Polymers NPP 60-908 Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -17.8 °C |
>= 26.7 ft-lb @Temperature -0.0400 °F |
ASTM D5420 |
Diamond Polymers NPP 60-908 Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -28.9 °C |
>= 26.7 ft-lb @Temperature -20.0 °F |
ASTM D5420 |
Diamond Polymers NPP 60-908 Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C3 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C4 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -17.8 °C |
>= 26.7 ft-lb @Temperature -0.0400 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C4 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C5 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -17.8 °C |
>= 26.7 ft-lb @Temperature -0.0400 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C5 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -28.9 °C |
>= 26.7 ft-lb @Temperature -20.0 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C5 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C8 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -28.9 °C |
>= 26.7 ft-lb @Temperature -20.0 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C8 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D5420-96 |
Solvay Engineered Polymers SEQUEL® E3000 HMS TPO
(discontinued **) Description: SEQUEL® E3000HMS thermoplastic olefinic elastomer (TPO) is designed for exterior and interior applications that require stiffness and durability. This extrusion-grade material is spec.. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420-96 |
Solvay Engineered Polymers SEQUEL® E3000 HMS TPO
(discontinued **) Description: SEQUEL® E3000HMS thermoplastic olefinic elastomer (TPO) is designed for exterior and interior applications that require stiffness and durability. This extrusion-grade material is spec.. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420-96 |
Solvay Engineered Polymers DEXFLEX® E160 TPO
(discontinued **) Description: DEXFLEX® E160 thermoplastic olefinic elastomer (TPO) is designed for extrusion applications that require thermal stability, excellent low-temperature properties, and good dimensional s.. |
|||
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D5420-96 |
Solvay Engineered Polymers SEQUEL® E2200 TPO
(discontinued **) Description: SEQUEL® E2200 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require low-temperature toughness and high rigidity. This pro.. |