Polymer Property : Dart Drop, Total Energy = 11.1 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 15.0 J

@Temperature 23.0 °C
11.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS
PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance.
Dart Drop, Total Energy 15.0 J

@Temperature 23.0 °C
11.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East)
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod..
Dart Drop, Total Energy 15.0 J

@Temperature 23.0 °C
11.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP ZX09022 PPE+PP (Europe-Africa-Middle East)
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod..
Dart Drop, Total Energy 15.0 J

@Temperature -30.0 °C
11.1 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA
High flow PPO+PA. Power distribution box applications.
Dart Drop, Total Energy 15.0 J

@Temperature -30.0 °C
11.1 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific)
High flow PPO+PA. Power distribution box applications.
Dart Drop, Total Energy 15.0 J

@Temperature 23.0 °C
11.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
Dart Drop, Total Energy 15.0 J

@Temperature 23.0 °C
11.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific)
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
Dart Drop, Total Energy 15.0 J

@Temperature 23.0 °C
11.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East)
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
Dart Drop, Total Energy 15.0 J

@Temperature 23.0 °C
11.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East)
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod..