Mechanical Properties Metric English Comments
Dart Drop, Total Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Dart Drop, Total Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific)
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Dart Drop, Total Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Dart Drop, Total Energy 70.0 J

@Temperature -30.0 °C
51.6 ft-lb

@Temperature -22.0 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Asia Pacific)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Dart Drop, Total Energy 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer
Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color.
Dart Drop, Total Energy 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Asia Pacific)
Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color.
Dart Drop, Total Energy 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color.
Dart Drop, Total Energy 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Dart Drop, Total Energy 70.0 J

@Temperature -20.0 °C
51.6 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Dart Drop, Total Energy 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4830 PBT+PC
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Dart Drop, Total Energy 70.0 J

@Temperature -20.0 °C
51.6 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4830 PBT+PC
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Dart Drop, Total Energy 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Dart Drop, Total Energy 70.0 J

@Temperature -20.0 °C
51.6 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Dart Drop, Total Energy 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Dart Drop, Total Energy 70.0 J

@Temperature -20.0 °C
51.6 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Dart Drop, Total Energy 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Dart Drop, Total Energy 70.0 J

@Temperature -20.0 °C
51.6 ft-lb

@Temperature -4.00 °F
ASTM D3763