Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Europe-Africa-Middle East) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 1000FC PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. NSF-51 certified for selected colors. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 1000R PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 1010F PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 1010FC PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 1010M PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 1010R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 2110R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 4000 PEI (Europe-Africa-Middle East) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), .. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM MD141 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East) Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM PW2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® VX8532 PBT+PET (Europe-Africa-Middle East) VALOX VX8532 is a 30% glassfiber reinforced, non blooming, flame retardant PBT+PET blend with excellent surface appearance and good ultrasonic weldability properties.This data was supplied by SABIC-.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 1000P PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. Resin is RoHS compliant. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM AUT200M PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C) with internal mold release.. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are re.. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Hardness, H358/30 | 140 MPa | 20300 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be sup.. |