Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips 1124 Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Impact Strength, Good Processability, Low Gels, Good Sealability, Medium Slip, High AntiblockApplications:Trash Bags and other LinersProcessing Condition.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips 2118 Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Impact Strength, Good Heat Seal Characteristics, Good Processability, Low GelsApplications:Trash bags and other linersProcessing Conditions: Extruder 6.3.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips 4522 LDPE Shrink and Heavy Duty Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Tensile Strength, Excellent Impact Strength, Very Good Tear Resistance, Very Good Abrasion Resistance, No Slip, No AntiblockApplications:Pallet Shri.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips 5622 LDPE Shrink and Heavy Duty Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Tensile and Impact Strength, Very Good Abrasion and Tear Resistance, Excellent Retention of Properties after Aging, Wide Range of Shrinkage Characte.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips 5625 LDPE Case Shrink and Bundling Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Superior Impact Strength, Good Abrasion and Tear Resistance, Good Sealing Properties, No Slip, High Antiblock, Easy Openability, Medium Coefficient of Frictio.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips 5658 LDPE Shrink and Bundling Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Impact Strength, Good Abrasion and Tear Resistance, Good Sealing Properties, No Slip, Medium Antiblock, Easy OpenabilityApplications:Shrink Wrap, Bundlin.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips MarFlex® 1122 Clarity, Liner Grade Film Resin Resin Type: HomopolymerCharacteristics: Good Impact, No slip, No antiblock, Good processability, Good sealabilityApplications:Liners, Trash bagsProcessing Conditions: Extruder 6.35 cm. Screw L/D Ra.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips MarFlex® 5613 LDPE Shrink and Heavy Duty Packaging Film Resin Resin Type: HomopolymerCharacteristics: Excellent Tensile Strength and Impact Strength, Very Good Abrasion Resistance and Tear Resistance, No Slip, High Antiblock, Medium Coefficient of Friction, Ea.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips MarFlex® 5619 LDPE Shrink and Heavy Duty Packaging Film Resin Resin Type: HomopolymerCharacteristics: Excellent Tensile and Impact Strength, Good Abrasion and Tear Resistance, Good Resistance to Blocking, Wide Range of Shrinkage Characteristics, Low Slip, Low .. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TX9003 LDPE Blown Film Extrusion Polyethylene TX9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance, good optical properties, and high stiffness. These characteristics provide, in some applications, down gaug.. |
|||
Secant Modulus, TD | 0.180 - 0.200 GPa | 26.1 - 29.0 ksi | Average value: 0.185 GPa Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Liner Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Liner Grade". Each property range of values reported is minimum and max.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | ASTM D882 |
Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Secant Modulus, TD | 0.180 GPa | 26.1 ksi | 2% Secant Modulus; ASTM-D882 |
Braskem TS9003 LDPE Blown Film Extrusion Polyethylene TS9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance along with good optical properties and high stiffness. These characteristics ensure the production of packag.. |