Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | |
ND Industries 560 Shaft & Bearing Retainer Retaining Compound High Temperature retainer for bushings and sleeves. Retains rotors to shaftsMeets military spec Mil-R-46082B Type II |
|||
Shear Strength | 13.8 MPa | 2000 psi | |
NextGen Adhesives G907-27 Structural Adhesive Description: NGAC G907-27 is a medium viscosity polyamide adhesive system utilized extensively in industrial and structural applications.Advantages and Applications: The NGAC G907-27 provides excell.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Al/Al, Tensile lap |
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Tensile lap, Al to Al |
Master Bond EP42-2LV Epoxy Resists Heat and Chemicals Description: Master Bond Polymer System EP42-2LV is a low viscosity room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring outstanding chemical resis.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Tensile lap, Al/Al |
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 301-2 Optically Transparent Epoxy Product Description: EPO-TEK® 301-2 is a two component optical, medical, and semiconductor grade epoxy resin, with low viscosity, long pot-life, and good handling characteristics.Advantages & Appli.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 323LP Epoxy Material Description: Longer pot life version of EPO-TEK® 353ND designed for semiconductor, hybrid, fiber-optic, hard-disk drive and medical applications.Information Provided by Epoxy Technology |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications. Advantages & Application Notes: This produ.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 360 Low Viscosity Optical Epoxy Adhesive Product Description: EPO-TEK® 360 is a two component, high-temperature grade epoxy for semiconductor, electronics, fiber optics and medical applications.Advantages & Application Notes: Built in col.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 360ST High Temperature Epoxy Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a slightly th.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 730 General Purpose Epoxy Product Description: EPO-TEK® 730 is a two component, thixotropic, room temperature-curing epoxy adhesive. Advantages & Application Notes: Excellent all purpose adhesive. Many uses in job shop and .. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Lap |
Epoxy Technology EPO-TEK® T7139 Glob Top Epoxy Product Description: EPO-TEK® T7139 is a two component, electrically insulating, encapsulating epoxy designed for semiconductor glob top applications and package assembly.Advantages & Application N.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Overlap, Al/Al, 20% Salt Spray 30 days @ 35°C; ASTM D1002-72 |
3M Scotch-Weld™ 1751 B/A Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1751 B/A is a gray, aluminum filled, two-part, room temperature curing structural adhesive.Information provided by 3M |
|||
Shear Strength | 13.8 MPa | 2000 psi | Overlap, Steel; ASTM D1002-64 |
3M Scotch-Weld™ CA50 Gel Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. High-viscosity, non-sag gel and less sensitive to acidic surfaces.Information provided by 3M |
|||
Shear Strength | 13.8 MPa | 2000 psi | Overlap, Galvanized Steel Okite degrease Hot dip |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 13.8 MPa @Temperature 49.0 °C |
2000 psi @Temperature 120 °F |
Overlap, Cohesive Failure |
3M Scotch-Weld™ DP810 Black Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Lap |
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Lap |
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Overlap, FR-4 Glass Epoxy |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 13.8 MPa | 2000 psi | cured |
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati.. |
|||
Shear Strength | 13.8 - 31.0 MPa | 2000 - 4500 psi | Average value: 20.6 MPa Grade Count:17 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Shear Strength | 13.8 MPa @Temperature -53.0 °C |
2000 psi @Temperature -63.4 °F |
Overlap, Etched Aluminum; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Tensile lap, Al/Al |