Mechanical Properties Metric English Comments
Shear Strength 8.62 - 11.0 MPa
1250 - 1600 psi
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
Shear Strength 8.62 - 10.3 MPa
1250 - 1500 psi
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works..
Shear Strength 8.62 - 10.7 MPa
1250 - 1550 psi
ITW Plexus Plexusâ„¢ MA557 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Long working time, non-sagging, excellent g..
Shear Strength 8.62 - 10.3 MPa
1250 - 1500 psi
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works.
Shear Strength >= 8.62 MPa
>= 1250 psi
Bond, Al to Al
Master Bond EP76M-1R Nickel Conductive Epoxy Adhesive
Description: Master Bond Polymer System EP76M-1R is a two component, nickel filled, electrically conductive adhesive for high performance bonding formulated to cure at room temperature or more rapid..
Shear Strength >= 8.62 MPa
>= 1250 psi
Plate Shear (Beam shear for 12.0 pcf products), L Direction, min
Hexcel® HexWeb® CR III 1/8-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 8.62 MPa
>= 1250 psi
Plate Shear (Beam shear for 12.0 pcf products), L Direction, min
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.0037 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 8.62 MPa
1250 psi
Lap
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy
Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotr..
Shear Strength 8.62 MPa
1250 psi
CRS Overlap, 100% RH at 49°C
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
Shear Strength 8.62 MPa
1250 psi
Overlap, Abraded Aluminum, 30 days tap water @ RT
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Shear Strength 8.62 MPa
1250 psi
Overlap, Lexan, Cohesive Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
Shear Strength 8.62 MPa
1250 psi
Overlap, 71°C 100% RH for 14 days, Mixed Mode of AF&CF
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 8.62 MPa

@Temperature 32.0 °C
1250 psi

@Temperature 89.6 °F
Overlap, Oak, 90% RH, Substrate/Adhesive Failure
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 8.62 MPa

@Temperature -55.0 °C
1250 psi

@Temperature -67.0 °F
Overlap
3M Scotch-Weld™ DP100 FR Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 FR is a two-part flame retardant (self-extinguishing) version of Scotch-Weld DP100. It meets the UL94 V-O Burn Test requirements and has a work life of 4-8 mi..
Shear Strength 8.62 MPa
1250 psi
Overlap, Acrylic
3M Scotch-Weld™ DP820 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Shear Strength 8.62 MPa

@Temperature 81.0 - 83.0 °C
1250 psi

@Temperature 178 - 181 °F
Minimum MMM-A-132 Requirement
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M
Shear Strength 8.62 MPa
1250 psi
Overlap, Abraded Aluminum, 30 days tap water @ RT
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M