Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 76.0 MPa | 11000 psi | ASTM D732 |
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Shear Strength | 76.0 - 79.0 MPa | 11000 - 11500 psi | Average value: 77.0 MPa Grade Count:3 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Shear Strength | 76.0 MPa | 11000 psi | as molded |
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Shear Strength | 76.0 MPa | 11000 psi | as molded |
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Shear Strength | 76.0 MPa @Temperature 22.0 °C |
11000 psi @Temperature 71.6 °F |
0° |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Shear Strength | 76.0 MPa | 11000 psi | IL; pr EN 2563 |
Hexcel® HexPly® 920CX-FM40J-6-42% 125°C Curing Epoxy Matrix High modulus carbon, Unidirectional, 165 g/m2Information provided by HexCel |
|||
Shear Strength | 76.0 MPa @Temperature 23.0 °C |
11000 psi @Temperature 73.4 °F |
DAM; ASTM D732 |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Shear Strength | 76.0 MPa | 11000 psi | ASTM D732 |
Ascend Performance Materials VYDYNE® R513 Nylon, 13% Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Shear Strength | 76.0 MPa | 11000 psi | ASTM D732 |
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |