Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 66.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 66.0 MPa
9570 psi
ILSS - Interlaminar; ASTM D2344
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System
EPOCYL™ NC R2HM-01 is a formulated epoxy based resin system for hot melt pre-preg and pressure molding processes, modified with our own Carbon Nanotubes (CNT), specifically developed to enhance the..
Shear Strength 66.0 MPa
9570 psi
ASTM D732
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin
Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov..
Shear Strength 66.0 - 75.0 MPa
9570 - 10900 psi
2mm/min.; IS 867-1963
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded
Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg..
Shear Strength 66.0 - 75.0 MPa
9570 - 10900 psi
IS 867-1963
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded
Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow ..
Shear Strength 66.0 - 76.0 MPa
9570 - 11000 psi
2mm/min.; IS 867-1963
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane..
Shear Strength 66.0 - 75.0 MPa
9570 - 10900 psi
2mm/min.; IS 867-1963
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni..
Shear Strength 66.0 - 75.0 MPa
9570 - 10900 psi
2mm/min.; IS 867-1963
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication ..
Shear Strength 66.0 MPa

@Temperature 23.0 °C
9570 psi

@Temperature 73.4 °F
ASTM D732
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con..