Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 60.0 MPa | 8700 psi | Die |
Lord Adhesives Thermosetâ„¢ ME-541 Underfill Encapsulant LORD Thermosetâ„¢ ME-541 encapsulant is an anhydride free, high purity, semi-conductor grade epoxy underfill product developed for the encapsulation of densely populated area array flip chip devi.. |
|||
Shear Strength | 60.0 MPa | 8700 psi | 0°, Short Beam |
Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, E-glass Balanced fabric 390 g/m2 Information provided by HexCel |
|||
Shear Strength | 60.0 MPa | 8700 psi | 0°, Short Beam |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 430 g/m2 Information provided by HexCel |
|||
Shear Strength | 60.0 MPa | 8700 psi | ILSS; EN2563 |
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/40%/193P/CHS-3K Fiber: HS Carbon, Plain Weave, 193 g/m2Information provided by HexCel |
|||
Shear Strength | 60.0 - 100 MPa | 8700 - 14500 psi | UD |
UBE Tyrannohex® Heat Resistant Composite Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe.. |
|||
Shear Strength | 60.0 MPa | 8700 psi | 0º, ILSS (Short Beam), RT, Dry; EN2563 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |
|||
Shear Strength | 60.0 MPa | 8700 psi | Warp ILSS, RT |
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix, M26T/50%/7581 Glass Fabric 300 gsmInformation provided by HexCel |
|||
Shear Strength | 60.0 MPa @Thickness >=5.00 mm |
8700 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good electrical and mechanical properties by continuous use, even at high temperatures. Very good chemical resistance. Engineering and insulation material in electrical mac.. |
|||
Shear Strength | >= 60.0 MPa | >= 8700 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications. High mechanical strength. Arc and tracking resistant. Flame retardant. Information provided by Hippe. |
|||
Shear Strength | >= 60.0 MPa | >= 8700 psi | IS 867-1963 |
Amity Thermosets ATM 123 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownMedium flow.. |
|||
Shear Strength | 60.0 - 70.0 MPa | 8700 - 10200 psi | IS 867-1963 |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Shear Strength | 60.0 - 65.0 MPa | 8700 - 9430 psi | IS 867-1963 |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Shear Strength | 60.0 - 70.0 MPa | 8700 - 10200 psi | IS 867-1963 |
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha.. |