Material Notes:
300 gsmInformation provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 400 MPa

@Temperature 80.0 °C
58000 psi

@Temperature 176 °F
Warp TS
410 MPa

@Temperature 23.0 °C
59500 psi

@Temperature 73.4 °F
Flexural Yield Strength 450 MPa

@Temperature 80.0 °C
65300 psi

@Temperature 176 °F
Warp
520 MPa

@Temperature 23.0 °C
75400 psi

@Temperature 73.4 °F
Flexural Modulus 16.5 GPa

@Temperature 80.0 °C
2390 ksi

@Temperature 176 °F
Warp
18.0 GPa

@Temperature 23.0 °C
2610 ksi

@Temperature 73.4 °F
Compressive Yield Strength 500 MPa
72500 psi
Warp, RT
Compressive Modulus 22.0 GPa
3190 ksi
Warp, RT
Shear Strength 60.0 MPa
8700 psi
Warp ILSS, RT
44.0 MPa

@Temperature 80.0 °C
6380 psi

@Temperature 176 °F
Warp ILSS
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month